Effects of Annealing on the Microstructures and Mechanical Properties of Cold-Rolled TB8 Alloy
The microstructure and mechanical properties of TB8 cold-rolled plate with a thickness reduction of 50% during annealing at different temperatures are investigated. The results show that annealing for 1 h belo...
-
Article
Grain Refinement Behavior of Accumulative Roll Bonding-Processed Mg-14Li-3Al-2Gd Alloy
Mg-14Li-3Al-2Gd sheets were prepared by four-layer accumulative roll bonding (FARB). The grain size of Mg-14Li-3Al-2Gd alloy is refined from 252.8 to 5.3 μm after 4 cycles FARB. The refinement can be mainly at...
-
Article
Formation and Corrosion Protection of Layered Double Hydroxide Film on Mg-4Li-3Al and Mg-14Li-3Al Alloys
Mg(OH)2/Mg-Al layered double hydroxide (LDH) films were prepared on the surface of single phase Mg-4Li-3Al (α-Mg phase) and Mg-14Li-3Al (β-Li phase) alloys by in situ hydrothermal in pure water with chemical-free...