Influence of Microstructural Homogenization on the Localized Deformation Behavior of Single-Crystal Ni-Based Superalloy, CMSX-4
CMSX-4 is a technically important Ni-based superalloy which is used for various niche applications in the aerospace industries, owing to its...
-
Microstructures and Mechanical Behaviors of Ni-Based Single-Crystal Superalloy DD90 Joints Brazed with a Co-Based Interlayer
A third-generation nickel-based single-crystal superalloy, DD90, was brazed with a Co-based filler alloy under vacuum conditions. The microstructural...
-
The effect of oxidation on microstructures of a Ni-based single crystal superalloy during heat-treatment and simulated service conditions
Understanding the oxidation of Ni-based single crystal (SX) superalloys is significantly important because oxidation can damage the microstructure...
-
On Synergistic Effects of Hierarchical γ′ Precipitates and Discontinuous Plastic Flow in a Ni-based Single Crystal Superalloy with an [001] Orientation
AbstractA discontinuous plastic flow is detected in a single-crystal superalloy with an [001] orientation during tensile tests over a wide...
-
Solid-State Joining of Dissimilar Single Crystal and Polycrystalline Ni-Based Superalloys Using Field-Assisted Sintering Technology
Field assisted sintering technology (FAST) was studied as a method to solid-state join a single crystal Ni-based superalloy (PW1429) to the same...
-
Atomistic Evolution of Hf2S/γ′ Interfaces in a Hf-containing Ni-based Single-Crystal Superalloy
The evolution of interfacial structures of needle-like sulfides in a Hf-containing Ni-based single-crystal superalloy has been studied with a...
-
Research on Finite Element Simulation and Recrystallization of Laser Shock Peened Nickel-Based Single-Crystal Superalloy
As the key material of aero-engine turbine blades, nickel-based single-crystal superalloys are in long-term service under high temperature, high...
-
Study on the relationship between TCP phase and AlN phase in a fourth-generation single-crystal superalloy
The enhanced mechanical properties of Ni-based single-crystal superalloys induced by refractory elements such as Re, Wo, Mo, etc. are essential for...
-
An In Situ X-ray Tomography Study on the Stress Corrosion Behavior of a Ni-Based Single-Crystal Superalloy
The present study was devoted to investigating the stress corrosion behavior of Ni-based single-crystal superalloys using in situ three-dimensional...
-
Change in Failure Behavior and Fatigue Life of Single-Crystal Ni-Based Superalloys Under Thermomechanical Fatigue Loading
This study discusses the thermomechanical fatigue (TMF) behavior of a first-generation Ni-based single-crystal superalloy. Tests were conducted for...
-
Composition design and microstructure of Ni-based single crystal superalloy with low specific weight—numerical modeling and experimental validation
Ni-based single crystal (SX) superalloys with low specific weight are essential for develo** aero engine turbine blades with great...
-
Effect of Magnetic Field Configuration on Stray-Crystal Formation with Different Platform Sizes during Directional Solidification of Single-Crystal Superalloy
The magnetic field is an effective means to control the solidification structure and the defects of metal and semiconductor crystals. This work...
-
Creep Durability of Ni-Base Single Crystal Superalloy Containing Pb Impurity
The effect of Pb on the creep properties of Ni-base single crystal superalloy was evaluated and compared with the reference data of polycrystalline...
-
Robust joining of FGH98 superalloy to DD5 single crystal by modulating interdiffusion behavior with Ni/high-entropy alloy hybrid interlayer
FGH98 superalloys and DD5 single crystals are highly desired to work together in high-temperature service environments. In this study, the FGH98-DD5...
-
Uniformity of the Dendritic Microstructure in Large-Sized Single-Crystal Superalloy Blades
The distribution of the dendrite arrays and the primary dendrite arm spacing (PDAS) in large-sized single-crystal superalloy blade was investigated...
-
High-temperature oxidation behavior of a single-crystal high-entropy superalloy strengthened by dense intermetallic nanoparticles
The oxidation behavior of a newly developed single-crystal L1 2 -strengthened Co-rich high-entropy superalloy, Co 41 Ni
35 Al 11.5 Ta 2.5 Cr 4 Ti 6 (at%), was... -
Tribological Behavior of a Shot-Peened Nickel-Based Single Crystal Superalloy at High Temperature
The tribological behavior of a nickel-based single crystal superalloy treated by shot-peening has been investigated. Friction tests under three...
-
Competitive oxidation behavior of Ni-based superalloy GH4738 at extreme temperature
A high thrust-to-weight ratio poses challenges to the high-temperature performance of Ni-based superalloys. The oxidation behavior of GH4738 at...
-
Oxidation behavior of Ni-based superalloy GH4738 under tensile stress
Revealing the oxidation behavior of superalloys is crucial for optimizing material properties and extending service life. This study investigated the...
-
Improvement of Oxidation Resistance for Ni-Base Single Crystal Superalloy TMS-238 by Suppression of Sb Segregation at Oxide/Substrate Interface Using CaO
Impurity Sb degrades the oxidation resistance of Ni-base superalloys after Al 2 O 3 crucible melting. The purpose of this study is to clarify the effect...