Article
Slurry Erosion Behaviour of Low-Temperature Liquid Nitrided 16Cr5Ni Martensitic Stainless Steel
Hydroturbine blades experience erosive wear during operations due to the presence of silt particles. The hydroturbine blades are fabricated from 16Cr5Ni martensitic stainless steels (16/5MSS). In order to miti...
-
Article
Studies on Enhancement of Silt Erosion Resistance of 13/4 Martensitic Stainless Steel by Low-Temperature Salt Bath Nitriding
Low-temperature salt bath nitriding of heat treated and tempered 13/4 Martensitic stainless steel (13/4HTT) was carried at 450 °C (N450) and 500 °C (N500) for 10 h each. The nitrided samples were characterized...