Article
Effects of Marker Size and Distribution on the Development of Kirkendall Voids, and Coefficients of Interdiffusion and Intrinsic Diffusion
Development of Kirkendall voids, and determination of interdiffusion coefficients, marker plane movement and intrinsic diffusion coefficients were investigated as functions of marker size and distribution usin...
-
Article
Phase Transformations and Microstructural Development in the U-10 Wt Pct Mo Alloy with Varying Zr Contents After Heat Treatments Relevant to the Monolithic Fuel Plate Fabrication Process
Decomposition of metastable, isotropic, body-centered cubic γ-phase in the U-10 wt pct Mo alloys with varying Zr contents was investigated as function of heat treatment parameters (i.e., temperature and time) rel...