Effect of mould baffle technology on stray grain formation in single crystal blades by integral fabrication based on 3D printing
Stray grains, the most serious casting defect, mainly occur in the platform because of the abrupt transition of the cross-section in the directional solidification of superalloy single-crystal blades. A new mo...
-
Article
Interlayer shear strength of single crystalline graphite
Reported values (0.2 MPa–7.0 GPa) of the interlayer shear strength (ISS) of graphite are very dispersed. The main challenge to obtain a reliable value of the ISS using conventional measuring methods was the un...