![Loading...](https://link.springer.com/static/c4a417b97a76cc2980e3c25e2271af3129e08bbe/images/pdf-preview/spacer.gif)
-
Article
Open AccessMorphological features of magnetorheological elastomer degradation under a natural weathering environment
It is well known in the field of materials science that a substance’s longevity is significantly influenced by its environment. Everything begins with the initial contact on a material’s surface. This influenc...
-
Chapter and Conference Paper
Using X-Ray Computed Tomography for Effective Porosity Characterisation in Additively Manufactured Metallic Parts
Common microscopy approaches are considered as destructive technologies for porosity characterization in metallic parts for various engineering components. They are not only time consuming, but also causes was...
-
Chapter and Conference Paper
A Review on Torque Performance for Different Type of Carrier Fluid in Magnetorheological Brake
Last two decades, the researcher is focused on increasing the braking torque of magnetorheological (MR) brake due to the insufficient braking torque to realize in commercial applications particularly vehicle a...
-
Article
Elimination of porosity in additively manufactured 316L stainless steel by high-pressure torsion
In metal additive manufacturing (AM), porosity is a major defect that could compromise their mechanical and functional performance. Very recently, high-pressure torsion (HPT) has emerged as an effective approa...
-
Article
Open AccessEffect of sample orientation on the microstructure and microhardness of additively manufactured AlSi10Mg processed by high-pressure torsion
For the first time, high-pressure torsion (HPT) was applied to additively manufactured AlSi10Mg built in two directions (vertical and horizontal) by selective laser melting (SLM), and the influence of extreme ...