    High-speed camera study of Stage III crack propagation in chemically strengthened glass

    Thermally or chemically strengthened glass is more resistant to damage and breakage compared to non-strengthened glass. Both strengthening mechanisms are based on incorporation of a compressive stress profile ...

    Zhongzhi Tang, Matthew B. Abrams, John C. Mauro, Leon R. Zoeller in Applied Physics A (2014)