Skip to main content

and
  1. No Access

    Article

    Rapid preparation of indium tin oxide sputtering targets by spark plasma sintering

    T. Takeuchi, T. Ishida, K. Ichikawa, S. Miyamoto in Journal of Materials Science Letters (2002)

  2. No Access

    Article

    Fabrication of silicon nitride nano-ceramics by spark plasma sintering

    T. Nishimura, M. Mitomo, H. Hirotsuru, M. Kawahara in Journal of Materials Science Letters (1995)

  3. No Access

    Article

    Reducibility of laterite ores

    The reducibility of several types of lateritic nickel bearing ores was investigated. The ores were reduced with hydrogen over a temperature range of 673 to 1273 K and reaction times from 5 to 80 minutes. The f...

    M. Kawahara, J. M. Toguri, R. A. Bergman in Metallurgical Transactions B (1988)