    Bi4Ti3O12-Based Piezoelectric Ceramics for High Temperature Applications

    High temperature piezoelectric ceramics based on WO3-doped Bi4Ti3O12 (WBIT) were prepared by two ways: chemical (hydroxide coprecipitation) and conventional oxides mixing. Sintering was carried out between 800°-1...

    M. Villegas, A. C. Caballero, C. Moure in Piezoelectric Materials: Advances in Scien… (2000)