Article
Photoluminescence Decay and Hydrogen Desorption of n-Type Porous Silicon
The decay under illumination of the photoluminescence (PL) intensity ofn-type porous silicon (PS) samples prepared by electrochemical etching has been investigated. We have found that the PL evolution with ill...