Article
A Simplified Hot-Tearing Criterion for Shape Castings Based on Temperature-Field Simulation
Current hot-tearing predictions for shape castings are suitable for well-investigated alloys with complete mechanical property databases, but are not applicable to newly developed alloys. This study proposed a...
-
Article
Effects of Gd and Zr additions on the microstructures and high-temperature mechanical behavior of Mg–Gd–Y–Zr magnesium alloys in the product form of a large structural casting
The microstructures, high-temperature mechanical properties, and fracture behavior of Mg–Gd–Y–Zr alloy components produced by low-pressure sand casting with different Gd and Zr contents, have been investigated...
-
Article
High cycle fatigue properties of cast Mg–xNd–0.2Zn–Zr alloys
The tensile and fatigue strength of cast Mg–xNd–0.2Zn–0.45Zr alloys (x = 0, 1, 2, 3 wt%) in both solution-treated (T4) and solution + 200 °C peak-aged (T6-PA) conditions were investigated in the present study. Th...
-
Article
High Cycle Fatigue of Cast Mg-3Nd-0.2Zn Magnesium Alloys
This paper investigates the high cycle fatigue properties of a recently developed high-strength cast magnesium alloy [Mg-3Nd-0.2Zn (all compositions in wt pct except when otherwise stated)] with varied Zr cont...
-
Article
Strengthening mechanisms in solution treated Mg–yNd–zZn–xZr alloy
A number of solution treated Mg–0.52Nd–0.08Zn–xZr (x = 0, 0.01, 0.03, 0.07, 0.12, and 0.14), Mg–yNd–0.08Zn–0.12Zr (y = 0, 0.17, 0.34, and 0.52) and Mg–0.52Nd–zZn–0.12Zr (z = 0, 0.08, 0.19, and 0.38) (at.%) cast a...
-
Article
Grain Refinement of AZ31 Magnesium Alloy by Titanium and Low-Frequency Electromagnetic Casting
The grain-refinement effects of titanium (Ti) additions and a low-frequency electromagnetic casting (LFEC) process on the AZ31 magnesium alloy have been investigated. It is shown that Ti has no effect on the f...