    Effect of mold and core preheating temperature on corrosion resistance of casting Al-12Si alloy U-shaped cooling channel

    Temperature has an important impact on the corrosion resistance of mold with cooling channels prepared by casting method. The effect of preheating temperature of the mold and the carbon fiber core on the rough...

    Guang-long Li, Jie Zhang, Meng-yu Wang, Rui-ming Su, Yang Cao in China Foundry (2023)

  2. Article

    Effect of secondary aging on microstructure and properties of cast Al-Cu-Mg alloy

    To obtain better comprehensive properties of cast Al-Cu-Mg alloys, the secondary aging (T6I6) process (including initial aging, interrupted aging and re-aging stages) was optimized by an orthogonal method. The...

    Rui-ming Su, Yong-xin Jia, Jian **ao, Guang-long Li, Ying-dong Qu in China Foundry (2023)

  3. Article

    Effect of TiO2 nano-ceramic particles on microstructure and mechanical properties of Al0.4CoCrFe2Ni2 high-entropy alloy

    Al0.4CoCrFe2Ni2 high-entropy alloys with different additions of TiO2 nano-ceramic particles (0, 1.25vol.%, 2.5vol.%, 3.75vol.% and 5vol.%, respectively) were prepared by using the vacuum arc melting method. The e...

    Hao Qi, Guang-long Li, Wei Zhang, Qing-yao Lü, Rong-de Li, Si-chen **e in China Foundry (2022)

  4. Article

    Effect of V and Sn on microstructure and mechanical properties of gray cast iron

    The cylinder liner is one of the important parts of a diesel engine. Gray cast iron is the main material for manufacturing cylinder liners due to its good casting performance, convenient processing performance...

    Yi-li Li, Rui-run Chen, Qi Wang, Wen-chao Cao, **n-xiu Wang, in China Foundry (2022)

  5. Article

    Glass formation in Fe-Cr-Zr-B-Mo alloys by tuning Nb addition

    Fe-based bulk metallic glasses (BMGs) with high boron content have potential application as a coating material used in the framework for storing spent nuclear fuels to support their safe long-term disposal. Th...

    Cong-ran Fu, Wei Zhang, Qing-chun **ang, Ying-dong Qu, Ying-lei Ren, Bo Yu in China Foundry (2021)

  6. Article

    Effect of melt cooling rate on glass transition kinetics and structural relaxation of Vit1 metallic glass

    The thin ribbons and the bulk cylindrical rods with diameters of 2 mm and 10 mm of the Vit1 metallic glass (MG) were prepared by the single roller melt spinning method and the copper mold injection casting met...

    Wei Zhang, Qing-chun **ang, Ying-dong Qu, Qing-feng Li, Ying-lei Ren in China Foundry (2021)

  7. Article

    Refinement and fracture mechanisms of as-cast QT700-6 alloy by alloying method

    The as-cast QT700-6 alloy was synthesized with addition of a certain amount of copper, nickel, niobium and stannum elements by alloying method in a medium frequency induction furnace, aiming at improving its s...

    Min-qiang Gao, Ying-dong Qu, Rong-de Li, Ke Jiang, Jun-hua You in China Foundry (2017)

  8. No Access

    Article

    Preparation of U-shaped curved holes by a casting method

    A technique to prepare U-shaped curved holes by a direct casting method was introduced, and U-shaped curved holes (with a diameter of 2 mm) with an aspect ratio of 35 were successfully prepared. A formula was ...

    Ying-Dong Qu, Gang Qin, Mei-Ling ** in The International Journal of Advanced Manu… (2016)

  9. Article

    Influence of Cr element on impact fracture process of ductile Ni-resistant alloyed iron at low temperature

    In this study, in order to investigate the influence of Cr element on the impact fracture process of ductile Ni-resistant alloyed iron at low temperature, different contents of Cr element were added to ductile...

    Ke Jiang, Ying-dong Qu, Jun-hua You, Rong-de Li, Qing-chun **ang in China Foundry (2016)

  10. No Access

    Article

    Low Temperature Impact Toughness and Fracture Analysis of EN-GJS-400-18-LT Ductile Iron under Instrumented Impact Load

    The impact toughness of EN-GJS-400-18-LT ductile iron was measured by Charpy V-notch impact test at temperature between — 80 and 20 °C. The fracture properties were tested under instrumented impact loading. Total...

    **n-ning Zhang, Ying-dong Qu in Journal of Iron and Steel Research International (2015)