  1. No Access

    Article

    Measurement of high temperature heat content of silicon by drop calorimetry

    Heat content of silicon has been measured in a temperature range of 700-1820 K using a drop calorimeter. Boron nitride was used as a sample crucible. The enthalpy of fusion and the melting point of silicon det...

    K. Yamaguchi, K. Itagaki in Journal of Thermal Analysis and Calorimetry (2002)

  2. No Access

    Article

    Magnetostructural phase transformation and shape memory effect of Fe-added Ni2MnGa films

    The magnetostructural phase transformation and shape memory effect (SME) of Fe-added Ni2MnGa films were investigated. The free-standing films were heat-treated at 1073 K for 3.6 ks and constraint-aged (CA) at var...

    M. Ohtsuka, J. Sekino, K. Koyama, T. Takagi in The European Physical Journal Special Topi… (2008)

  3. Article

    Open Access

    The Physics of the B Factories

    A. J. Bevan, B. Golob, Th. Mannel, S. Prell in The European Physical Journal C (2014)